MAGNETIC COMPOUNDS FOR EXTRUSION, INJECTION MOULDING AND CALENDERING


Magnetic compounds are made by embedding a Barium or Strontium ferrite reinforcement into a polymer-elastomer matrix using open or closed mixers. The quamtity of ferrite powder in the compound may be higher than 90% of total weight. Ilpea supplies both isotropic and anisotropic compounds, which can be extruded, calendered or injection moulded to make finished products, such as:

1) Flexiblle magnetic profiles for refrigerator door gaskets

Properties of isotropic compounds
type Ferrite Br (G) bHc (Oe) jHc (Oe) (BH) max
(MGOe)
Durezza
(ShD)
F02-KRQ Barium > 1400 > 1100 > 2000 > 0,4 60 - 80
F02-ERM Barium > 1450 > 1150 > 2000 > 0,4 60 - 80
F02-MOB5 Barium > 1500 > 1100 > 2000 > 0,45 40 - 60
SG1 Barium/Strontium > 1700 > 1500 > 2700 > 0,7 50 - 70
SG2 Barium/Strontium > 1800 > 1500 > 2700 > 0,7 50 - 70
SG8 Strontium > 1650 > 1100 > 1800 > 0,5 > 40
MF11 Strontium > 2000 > 1500 > 2700 > 0,8 50 - 70
(Values measured according to the ILPEA method)
Extruded isotropic and anisotropic magnetic profiles. For use on refrigerator doors, shower enclosures, display cabinets, etc.
immagine
2) Flexible high-energy anisotropic magnets, which are used to make electric motors, the control panels of elevators, promotional gadgets, magnetic displayers, etc.
 
Properties of anisotropic compounds
Type Ferrite Br (G) bHc (Oe) jHc (Oe) (BH) max
(MGOe)
Durezza
(ShD)
ZETA 5 Barium/Strontium > 2200 > 1800 > 2500 > 1,2 40 - 60
ZETA 18 Barium/Strontium > 2100 > 1800 > 2500 > 1,1 35 -55
LEV 05 Barium > 2350 > 2050 > 2400 > 1,3 > 15
LEV 04 Barium > 2450 > 2050 > 2400 > 1,4 > 15
(Values measured according to the ILPEA method).
Extruded anisotropic magnetic profiles. For use on magnetic encoders.
immagine
3) Rigid isotropic or anisotropic magnets, 3) primarily made by injection moulding and used as an alternative to the flexible ones.

Properties of the compounds for injection moulding
Tipo Ferrite Br (G) bHc (Oe) jHc (Oe) (BH) max
(MGOe)
Legante
I08-N85 Barium > 2400 > 2000 > 3000 > 1,35 PA 6
I08-N87 Barium > 2800 > 2000 > 2400 > 1,8 PA 6
I08-N88 Barium > 2700 > 2000 > 2400 > 1,75 PA 6
I08-N01 Strontium > 2550 > 2000 > 2700 > 1,6 PA 11/12
I08-N05 Strontium > 2700 > 2000 > 2400 > 1,75 PA 11/12
(Values measured accordino to the ILPEA methoid).
Extruded anisotropic magnetic profiles. For use on the control panels of elevators, on electric motors, etc.
immagine